000 01693cam  2200325za 4500
0019.865025
003CaOODSP
00520221107161711
007cr |||||||||||
008181121s1975    onc    #ot   f|0| 0 eng d
040 |aCaOODSP|beng
041 |aeng|bfre
043 |an-cn---
0861 |aM38-13/76-4E-PDF|zM38-13/76-4
1001 |aMcDonald, A. G.
24514|aThe preparation of mica cylinders for measurement of thermal conductivity |h[electronic resource] / |cA. G. McDonald and V. V. Mirkovich.
260 |a[Ottawa] : |bEnergy, Mines and Resources Canada, |c1975.
300 |aii, 12 p.
4901 |aCANMET report ; |v76-4E
500 |aCover title.
500 |a"December 1975."
504 |aIncludes bibliographic references.
520 |a"Measurements of thermal conductivity parallel with the basal {001} cleavage planes of the industrially important mica minerals have not been made in the past because of the difficulty of sample preparation. A method was devised to produce cylindrical mica specimens, 25.4 mm in diameter x 25.4 mm high, suitable for use in a comparative method apparatus for measurement of thermal conductivity. The mica cylinders can be prepared so that the planes of cleavage are either parallel or perpendicular to their longitudinal axis"--Summary, p. i.
546 |aIncludes summary in French.
69207|2gccst|aMinerals
69207|2gccst|aScientific research
7001 |aMirkovich, V. V.
7101 |aCanada. |bEnergy, Mines and Resources Canada.
830#0|aCANMET report ;|v76-4E.|w(CaOODSP)9.852792
85640|qPDF|s1.99 MB|uhttps://publications.gc.ca/collections/collection_2018/rncan-nrcan/m38-13/M38-13-76-4-eng.pdf