Flotation of uranium ores from the Elliot Lake area, Ontario / by W.R. Honeywell. : M34-20/2E-PDF
"The method and results of a series of flotation tests on several Elliot Lake uranium ores are given. The reagents used were NaOH and Na2SiO3 in a desliming step, and tall oil fatty acid, Acintol FA-1 or FA-2, was used as collector. The average recovery obtained was 92% in about 55% of the weight. The leach feed was up-graded from 0.1 to about 0.2% U308. The cost of the flotation reagents would be 25 to 30 cents per ton. A saving of about 20 cents per lb of uranium would be effected."--Abstract.
Lien permanent pour cette publication :
publications.gc.ca/pub?id=9.835497&sl=1
| Ministère/Organisme |
|
|---|---|
| Titre | Flotation of uranium ores from the Elliot Lake area, Ontario / by W.R. Honeywell. |
| Titre de la série |
|
| Type de publication | Monographie - Voir l'enregistrement principal |
| Langue | [Anglais] |
| Format | Texte numérique |
| Document électronique | |
| Note(s) |
|
| Information sur la publication |
|
| Auteur / Contributeur |
|
| Description | 8 p. : graphs. |
| Numéro de catalogue |
|
| Descripteurs |
Demander des formats alternatifs
Pour demander une publication dans un format alternatif, remplissez le formulaire électronique des publications du gouvernement du Canada. Utilisez le champ du formulaire «question ou commentaire» pour spécifier la publication demandée.Détails de la page
- Date de modification :