Uranium in alloy steel / C.E. Makepeace. : M38-1/129-1964E-PDF
"The effect on the mechanical properties at room temperature and at elevated temperatures, of adding uranium to alloy steel in plate and sheet form, was investigated in thirty-two factorial experiments. Statistically significant results indicate that uranium form a stable compound, probably uranium monocarbide, which is not affected by prior heat treatment. Adding less than one-half per cent uranium was observed to result in an increase in the time to reach 0.1% creep strain and a decrease in the susceptibility to hot cracking in alloy steel sheet"--Abstract.
Lien permanent pour cette publication :
publications.gc.ca/pub?id=9.869418&sl=1
| Ministère/Organisme |
|
|---|---|
| Titre | Uranium in alloy steel / C.E. Makepeace. |
| Titre de la série |
|
| Type de publication | Monographie - Voir l'enregistrement principal |
| Langue | [Anglais] |
| Format | Texte numérique |
| Document électronique | |
| Note(s) |
|
| Information sur la publication |
|
| Auteur / Contributeur |
|
| Description | 1 online resource (x, 67 pages) : figures. |
| Numéro de catalogue |
|
| Descripteurs |
Demander des formats alternatifs
Pour demander une publication dans un format alternatif, remplissez le formulaire électronique des publications du gouvernement du Canada. Utilisez le champ du formulaire «question ou commentaire» pour spécifier la publication demandée.Détails de la page
- Date de modification :